Thermoelectric Power and Resistivity of Chromium-Rich CrFe Alloys between 25° and 1000°C

Abstract

A study has been made of the thermoelectric powers (S) and electrical resistivities (ρ) of CrFe alloys over the concentration range 0 to 48.2 at. % Fe and temperature (T) range from 25° to 1000°C. The plots of S vs T and ρ vs T move in an orderly progression from that of pure Cr to the curve for the Cr51.8Fe48.2 alloy with no anomalies occurring. One might think that S should change sign as the alloy concentration passed through the region where Beck et al. observed their ``spike'' in the electronic specific heat, but no such phenomenon was observed.

Document Details

Document Type
Pub Defense Publication
Publication Date
Sep 01, 1967
Source ID
10.1063/1.1709030

Entities

People

  • John E. Cox
  • William H. Lucke

Organizations

  • United States Naval Research Laboratory

Tags

Fields of Study

  • Materials science

Readers

  • Approximation Theory.
  • Materials Science and Engineering.
  • Superconducting Magnet Technology

Technology Areas

  • Microelectronics