Modification of commercial boron carbide powder using Rapid Carbothermal Reduction

Abstract

Non‐uniform morphology and existence of free carbon are two main problems for commercial boron carbide powders. This work proposes a method for eliminating free carbon and changing the morphology of commercial powders using Rapid Carbothermal Reduction (RCR) process. Free carbon is eliminated from commercial boron carbide powders and morphology is evolved to less angular shapes with limited particle size growth. Commercial and modified powders were densified by Spark Plasma Sintering at 1900°C with 0, 5, and 20 minutes dwell. Despite the particle size growth, modified boron carbide powders reached >99% TD with shorter dwell times compared with commercial starting powders. Improved microhardness observed with dense modified samples as a result of enhanced morphology and increased twinning.

Document Details

Document Type
Pub Defense Publication
Publication Date
Oct 29, 2018
Source ID
10.1111/ijac.13130

Entities

People

  • M Fatih Toksoy
  • Richard A Haber

Organizations

  • Rutgers University
  • United States Army Research Laboratory
  • İzmir Institute of Technology

Tags

Fields of Study

  • Materials science

Readers

  • Powder metallurgy of Titanium alloys.
  • Thin Film Deposition Science.