SOVIET PRECIPITATION-HARDENABLE STAINLESS STEELS
Abstract
T e article suggests a different thermomechanical method of treatment for X17H7YU steel (Armco 17-7PH). According to present practice this steel is subjected to a 4-step heat treatment. It is first solution-annealed at 1100 C for 2 hr and air cooled. It is then conditioned twice at 700 C for 2 hr followed each time by air cooling. Finally, it is aged at 600 C for 4 hr and air cooled. Treated in this manner, X17H7YU HAS A NOTCH TOUGHNESS OF %-* KG-M/SQ CM AND A HARDNESS OF Rockwell C. The suggested thermomechanical treatment consists of the same solution annealing at 1100 C for 1-2 hr, followed by brine cooling, cold rolling (compression) at room or sub-zero temperature, and aging at 450-600 C followed by brine cooling. This method is especially suitable for parts where cold working is one of the last operations. (Author)
Document Details
- Document Type
- Technical Report
- Publication Date
- Jul 18, 1961
- Accession Number
- AD0261449
Entities
Organizations
- Library of Congress