TUNGSTEN EXTRUSION PROGRAM

Abstract

Ingots of W-3% Mo alloy were arc-melted by various electrode preparation techniques, melt rates and crucible sizes to optimize as-cast ingot quality. Ingots were evaluated for purity, soundness, structure and sidewall cleanup. Preliminary extrusions were made with two 6.55-in.-diam. billets at 2.8:1 reduction ratio and 3.725-in.-diam. billets at 11:1 and 17:1 reduction ratios at temperature above 3500F. Extrusion equipment and accessory tooling is discussed. Fine grained, low interstitial ingots were obtainable by blending, isostatic pressing to 1 to 2.5-in.-diam. rods, hydrogen sintering, mechanically joining and single arc-melting with dc straight polarity at a melt rate of less than 2 lb/min with magnetic stirring coil reversal. (Author)

Document Details

Document Type
Technical Report
Publication Date
Aug 24, 1961
Accession Number
AD0266713

Entities

People

  • A.e. Riesen
  • James Wong

Tags

DTIC Thesaurus Topics

  • Arc Melting
  • Blending
  • Crucibles
  • Electrodes
  • Extrusion
  • Fabrication
  • Hydrogen
  • Isostatic Pressing
  • Material Forming Processes
  • Materials Processing
  • Melting
  • Melts
  • Mixing
  • Polarity
  • Sintering
  • Transition Temperature

Fields of Study

  • Materials science

Readers

  • Metallurgy