MATERIAL-HIGH TEMPERATURE ADHESIVE-AEROBOND 500-PRELIMINARY EVALUATION OF PROPERTIES
Abstract
The lap shear strength of Aerobond-500-bonded 17-7 PH TH-1050 stainle s steel specimens was determined and found to be 355 psi lower than the values reported by the manufacturer when tested at 500 F after aging 100 hours at 500 F. (Author)