TUNGSTEN SHEET ROLLING PROGRAM

Abstract

Rolling and evaluation of the Phase III material has been completed. The effect of various processing parameters on work-ability and final properties is documented. Significant conclusions are: (1) extrusion to rounds or to rectangular cross-section sheet bar can be accomplished equally well, (2) initial rolling of extruded or extruded and forged product can be and is best accomplished in the temperature range of 2300 F, (3) in order to achieve the lowest ductile-brittle transition, final rolling temperatures should not exceed 1550 F, and (4) cross rolling improves both the longitudinal and the transverse bend and tensile properties. (Author)

Document Details

Document Type
Technical Report
Publication Date
Nov 01, 1962
Accession Number
AD0289065

Entities

People

  • W.j. Schoenfeld

Tags

DTIC Thesaurus Topics

  • Ductile Brittle Transition
  • Extrusion
  • Fabrication
  • Material Forming Processes
  • Materials
  • Materials Processing
  • Mechanical Properties
  • Mechanical Working
  • Tensile Properties
  • Test And Evaluation
  • Transitions
  • Transverse
  • Tungsten

Fields of Study

  • Materials science

Readers

  • Metallurgy