MATERIAL - ADHESIVE - FMS-0016 (PLASTILOCK 620-626) - LAP SHEAR SPECIMENS OF - ADHESIVE ALLOWABLES ON - TESTS FOR
Abstract
Slow uninterrupted load rates had no effect on bond strength of FMS-0016 adhesive bonded specimens with 0.5, 1.0 and 1.63 in. overlaps when tested at -67, 80, 180 and 260 F. The bond strengths of FMS-0016 adhesive test specimens were affected when tested at 260, 180 and 80 F by a loss in strength when held for interrupted and extended load periods at 75 and 90% of the predetermined ultimate load levels of the particular overlap specimens. The bond strength of FMS-0016 adhesive at -67 F was not affected when held for interrupted and extended load periods at the predetermined ultimate load level for .50, 1.0 and 1.63 inch overlap specimens.