THE EFFECT OF SURFACE DECARBURIZATION ON PROTOTYPE MISSILE CASES

Abstract

Progress is reported on the fabrication and hydrotesting of each of three types of decarburized prototype cases, namely: MBMC 1 and Super Tricent steel welded cases, Super Tricent seamless cases, and Super Tricent seamless cases with bonded end rings. Test results of MBMC 1 welded seam cases tabulated and graphically illustrated are shown to correlate with the laboratory specimen data gathered during the 1961 decarburization study. Also, test results of bonded uniaxial and biaxial stress specimens are given which indicate that the target bonded joint strength of 15,000 pounds per peripheral inch (3750 psi) established for the prototype bonded end ring case can be achieved. (Author)

Document Details

Document Type
Technical Report
Publication Date
Nov 15, 1962
Accession Number
AD0290559

Entities

People

  • D.p. Thomason
  • E.s. Mills

Tags

DTIC Thesaurus Topics

  • Biaxial Stresses
  • Bonded Joints
  • Dealloying
  • Fabrication
  • Joints
  • Material Forming Processes
  • Materials Processing
  • Mechanical Working
  • Prototypes
  • Stresses

Readers

  • Mechanical Engineering/Mechanics of Materials.
  • Metallurgy