MATERIAL - ADHESIVES - STRUCTURAL - METLBOND 4021. EFFECT OF GENTIAN VIOLET DYE ON TENSILE SHEAR STRENGTH

Abstract

The addition of 0.1% gentian violet to Metlbond 4021 adhesive primer was evaluated with respect to its effect on the strength of metal to metal bonds. Tensile-shear tests were made to compare tinted with un-tinted primers used in the preparation of joints which were bonded at 275 F under a pressure of 100 psi. The comparative test results showed that the dye did not adversely affect the Metlbond 4021 primer.

Open PDF

Document Details

Document Type
Technical Report
Publication Date
Jul 26, 1957
Accession Number
AD0407620

Entities

People

  • M. C. Miyaji
  • V. Lintvedt
  • W. M. Sutherland

Organizations

  • General Dynamics

Tags

DTIC Thesaurus Topics

  • Adhesives
  • Creep Tests
  • Dyes
  • Dynamics
  • Extensometers
  • Humidity
  • Identification
  • Indicator Dyes
  • Materials
  • Measurement
  • Shear Strength
  • Shear Tests
  • Surface Finishing
  • Tapes

Readers

  • Chemistry (specifically Chemical Fluorescence)
  • Surface Coatings Technology.