REFRACTORY ALLOY FOIL ROLLING DEVELOPMENT PROGRAM - PHASE III.
Abstract
The processing of three Nb-base alloys and two Ta-base alloys from ingot to 0.100 in. thick x 12 in. wide sheet is described. The alloys were Nb-10%W-1%Zr-0.1%C (D-43), Nb-5%Mo-5%V-1%Zr (B-66), Nb-10%W-2-1/2%Zr (Nb-752), Ta-10%W, and Ta-8%W-2%Hf (T-111). The operations involved were: extrusion, hot-rolling, conditioning, annealing, and cold-rolling. Rolling of small sheets of pure W (0.060 in. thick and below) is described.