MECHANICAL AND PHYSICAL PROPERTIES OF TZM MOLYBDENUM ALLOY SHEET OF TUNGSTEN SHEET

Abstract

Tensile tests were conducted on recrystallized 0.060 in. and 0.100 in. tungsten sheet from room temperature up to 3500F. Notched- and unnotched- tensile tests were conducted on the 0.060 in. tungsten sheet in the optimum and recrystallized connditions at moderately elevated temperatures (9900F and below) to determine the notched-tensile, brittle-ductile transition temperature. Tensile tests were conducted on recrystallized 0.060 in. and 0.100 in. tungsten sheet from room temperature up to 3500 F. Notchedand unnotched- tensile tests were conducted on the 0.060 in. tungsten sheet in the optimum and recrystallized conditions at moderately elevated temperatures (900 F and below) to determine the notched-tensile, brittle-ductile transition temperature. Tensile tests were completed on the 0.020 in., 0.040 in. and 0.060 in. TZM temperatures for these tests ranged from room temperature to 3000F.

Open PDF

Document Details

Document Type
Technical Report
Publication Date
Sep 30, 1964
Accession Number
AD0606310

Entities

People

  • Clifford L. Dotson
  • P. G. Adams

Organizations

  • Southern Research

Tags

Communities of Interest

  • Air Platforms
  • Weapons Technologies

DTIC Thesaurus Topics

  • Air Force
  • Aircrafts
  • Bearing Strength
  • Ductility
  • Elastic Properties
  • Engineering
  • Materials
  • Modulus Of Elasticity
  • Molybdenum
  • Molybdenum Alloys
  • Physical Properties
  • Reduction Of Area
  • Strain Rate
  • Tensile Properties
  • Tensile Strength
  • Transition Temperature
  • Transitions

Fields of Study

  • Materials science

Readers

  • Metallurgy