INFLUENCE OF IRON ON PHASE COMPOSITION, STRUCTURE, AND PROPERTIES OF A HEAT RESISTANT NICKEL-CHROMIUM-TUNGSTEN ALLOY,

Abstract

The alloy EI868 was heated to 1200C for 5 min. and then cooled in water or air. Alloy EI868 hardened during aging owing to the formation of the dispersed phases: carbides M23C6, solid solns. of tungsten in chromium, or intermetallic phase Fe2W. In alloys contg. Fe greater than or equal to 20% the alpha phase was formed. (Author)