RESISTANCE OF RUBBERS TO TROPICAL AND TEMPERATE CLIMATES,

Abstract

Seven rubbers, fluorinated rubber, neoprene ILA, PVC/nitrile rubber blend, ethylene/propylene/diene terpolymer, natural rubber, neoprene WRT and nitrile rubber, have been exposed outdoors in a stressed and unstressed condition on four sites - a temperate site and three tropical sites (hot/wet cleared, hot/wet jungle and hot/dry desert). The tensile strength, elongation at break and modulus were measured after 3, 6, 12 and 27 monthly intervals. The results show that ethylene/propylene/diene terpolymer, Viton and neoprene WRT were the least affected by exposure to temperate and tropical conditions. (Author)

Document Details

Document Type
Technical Report
Publication Date
Jan 01, 1969
Accession Number
AD0687223

Entities

People

  • A. L. Stokoe
  • B. L. Hollingsworth
  • D. J. Evans
  • K. J. Ledbury

Tags

DTIC Thesaurus Topics

  • Alkenes
  • Copolymers
  • Ethylenes
  • Natural Rubber
  • Neoprene
  • Nitrile Rubber
  • Propenes
  • Rubber
  • Tensile Strength

Readers

  • Polymer Science and Engineering.
  • Surface Coatings Technology.