Abstract
Phenol alkylated with polymer distillate was heated with anhydrous chloral in naphtha solution at 80 degrees 2.5 hrs., and the product heated with phosphorus pentasulfide 1.5 hrs. at 100 degrees and 5-6 hrs. at 120 degrees, dissolved in naphtha, and filtered to remove excess phosphorus pentasulfide. Removal of the solvent in vacuo gave the additive. Solution (3 percent) in various oils have antifriction and antiwear properties superior to those of comparitive additives. (Author)