Synthesis of Co-Imide-Quinoxalines,

Abstract

Phenylated, ordered imide-quinoxaline copolymers of high oxidative-thermal stability were prepared by one-step solution condensation of aromatic tetraamines with N,N'-bis(4-benzilyl)pyromellitimide. Polymerization in m-cresol leads to high molecular weight polymers that remain soluble. Thermal gravimetric analysis and isothermal decomposition at 400C shows that these polymers are as stable as polyimides or polyquinoxalines. The polymer decomposition temperatures range between 495 and 550C, depending upon structure. Also, the rate of isothermal decomposition at 400C in air showed a strong dependency of weight loss on structure. Tough films were cast from solution. (Author)

Document Details

Document Type
Technical Report
Publication Date
Jul 20, 1970
Accession Number
AD0713886

Entities

People

  • J. M. Augl

Organizations

  • Naval Ordnance Laboratory

Tags

DTIC Thesaurus Topics

  • Body Weight
  • Condensation
  • Copolymers
  • Decomposition
  • Gravimetric Analysis
  • Molecular Weight
  • Polymerization
  • Polymers
  • Quinoxalines
  • Thermal Stability
  • Transition Temperature

Fields of Study

  • Chemistry

Readers

  • Polymer Science and Technology

Technology Areas

  • Microelectronics