Properties of DEXSIL 300 Rubbers.
Abstract
The physical and elastomeric properties of several DEXSIL 300 (10-SiB-3) samples were investigated. Modulus-temperature studies were used to determine the glass transition temperature, the melting temperature, and the oxidative crosslinking temperature. Stress relaxation in air at elevated temperatures was used to compare the oxidative stability of the various formulations. (Author)
Document Details
- Document Type
- Technical Report
- Publication Date
- Mar 01, 1972
- Accession Number
- AD0739723
Entities
People
- Arthur V. Tobolsky
- Robert M. Mininni
Organizations
- Princeton University