Abstract
The report describes a method for increasing the sensitivity of positive color film in processing by adding potassium chloride to the developer. The implementation of this method in industry allowed the processing of low-sensitivity film without reducing the speed of the copier and increasing the voltage of the printing lamp. It was possible to increase the sensitivity of TSP-8R film 1.5-2 times by using potassium chloride developer.