Program to Develop High Strength Aluminum Powder Metallurgy Products. Phase 4A - Vacuum Process Verification
Abstract
Six P/M alloy-powders were prepared for this vacuum-preheat process verification. P/M 2-in. diameter extruded rod for extrusion evaluation was fabricated from vacuum preheated and hot pressed (VAC-preheat) compacts. Camparison ingot metallurgy (I/M) 7050 extrusions were also prepared. Preliminary test results show P/M alloys MA86, MA87, MA89 and MA67 developed good transverse fracture toughness and ductility, with transverse fracture toughness comparable to that achieved in VAC-preheat MA83 alloy. This verified the reproducibility of the fracture toughness improvement previously indicated for VAC-preheat over inert-gas (FCE) preheat. P/M 4-in. diameter extruded stock for die forging was fabricated from VAC-preheated 140-lb compacts. Comparison I/M 7050 extruded rod was also prepared.
Document Details
- Document Type
- Technical Report
- Publication Date
- Oct 12, 1972
- Accession Number
- AD0904979
Entities
People
- W. S. Cebulak
Organizations
- Alcoa