Synthetic Mooring Line Tensile Testing Procedure.

Abstract

This report describes an effort to determine whether or not a tensile test procedure is necessary that will provide commonality among tensile tests of synthetic lines of all materials, diameters and lengths. A relationship was derived that relates material stiffness, diameter, and sample lengths to the strain rate during a tensile test. A first order experiment was conducted in which synthetic lines were tensile tested at various strain rates to determine to what degree tensile strength is affected by strain rate. Results show that the dispersion among individual data points overshadows the general trend of any strain rate effect and negates the need for a specific relationship. It is recommended that the strain rate be kept below 5 millistrains per second because the data points in that range are less disperse and the results derived from them should be more reliable. Some variation was observed between manufacturer's rated breaking strength and the test data. Although there are exceptions, a variation in strain rate generally has an insignificant effect on elongation at failure, spring constant and unit energy absorption.

Open PDF

Document Details

Document Type
Technical Report
Publication Date
Sep 01, 1975
Accession Number
ADA035388

Entities

People

  • Kenneth R. Bitting

Organizations

  • [Means, goals and clinical aims of physioradiological methods of examination.]

Tags

DTIC Thesaurus Topics

  • Absorption
  • Commonality
  • Diameters
  • Dispersions
  • Elongation
  • Materials
  • Physical Properties
  • Stiffness
  • Strain Rate
  • Tensile Strength
  • Tensile Testing

Readers

  • Mechanical Engineering/Mechanics of Materials.
  • Systems Analysis and Design