Temper Embrittlement in 4140 Seamless Tubing
Abstract
In November 1976, several 155mm Howitzer M185 split rings failed during various stages of manufacture. A failure analysis consisting of metallography, SEM, and mechanical testing, was undertaken. This investigation concluded that the heat treatment was responsible for embrittling the steel, thereby causing the failures. Furthermore, it was shown that the required hardness could not be achieved without seriously compromising the toughness of this material.
Document Details
- Document Type
- Technical Report
- Publication Date
- Nov 01, 1977
- Accession Number
- ADA051294
Entities
People
- Peter Thornton
- Steve Tauscher
Organizations
- United States Army Armament Research, Development and Engineering Center