High Contrast CRT.
Abstract
Sixteen faceplates were completed and characteristic optical data was recorded. The difficulties in production result from the properties of the faceplate glass limiting the maximum temperature of the La2O2S heat treatment. The optimum fabrication techniques, with this limitation, produced quality faceplates. (Author)