Bulk Nanocomposite LaCo5/LaCo13 Magnets (POSTPRINT)
Abstract
The effects of processing parameters and composition on the magnetic properties and microstructure of nanocrystalline La-Co-based hard magnetic materials were investigated. Bulk nanocomposite LaCo5/LaCo13 magnets were fabricated by mechanical alloying of LaCo5 and La2Co7 powder mixtures and subsequent hot pressing at 580-810 deg C. A high coercive field (Hc) of over 16 kOe with a smooth demagnetization curve was obtained in a composition range of 25-30 wt. % La2Co7 when hot-pressed at 660-760 deg C. Microstructural investigations indicated that the magnets consist of a primary LaCo5 phase with grain sizes of 200-400 nm, coexisting with 20-100 nm grains of LaCo13 located both at the grain boundaries and within the hard LaCo5 grains.
Document Details
- Document Type
- Technical Report
- Publication Date
- Aug 01, 2012
- Accession Number
- ADA566254
Entities
People
- John Horwath
- Meiqing Huang
- Yuhui Shen
- Zafer Turgut
Organizations
- University of Dayton