Room Temperature Cured Elastomer.

Abstract

Hydroxy terminated polybutadiene is reacted with naphtyl-potassium and 1-bromo-2,4-pentadiene in successive steps to form a bis(1,3-pentadienyl ether) derivative. Then the bismaleimide of dimer diamine is added to the polybutadiene derivative whereby a room temperature cure to an elastomer is achieved. (Author)